The final firing temperature affected translucency, producing either perceptible or imperceptible differences between translucency levels and firing cycles. HT, MT, and HT-MT specimens generally showed lower BFS, suitable for adhesively cemented single-unit restorations, whereas other translucency levels may also be applicable for 3-unit prostheses, excluding molar teeth. Although Weibull moduli were similar, LT, MO, HT-LT, and HT-MO specimens generally had higher characteristic strength, indicating greater reliability.