Strength-ductility synergy and multiscale particle-solute interaction mechanisms in Al-Cu composites reinforced by TiC/TiB2 nanoparticles

View Full Paper
KJKaixi JiangWYWei YuZZZengshuo Zhang

Key Points

  • The tensile strength of the Al-Cu composites reached 543 MPa, indicating significant strength improvements.
  • Compared to the Al-Cu alloy, the grain size was reduced by 92.7%, highlighting the refinements achieved.
  • A multiscale modeling approach was established to simulate dendritic growth and solute distribution.
  • Orowan strengthening is the dominant mechanism contributing to the enhanced strength of the composites.

Abstract

• TiC/TiB 2 refines Al composite grains 92.7%. • The maximum volume of Al 2 Cu is refined by 96.7% • Diffusion-blocking model shows particle–dendrite interactions. • Heat-flow-solute and phase-field model reveals segregation behavior. This work proposes a novel manufacture method to enhance t1%he strength–ductility synergy of Al–Cu alloys by incorporating TiC/TiB 2 particles. The composites were fabricated using an in-situ synthesized Al-30TiC/TiB 2 master alloy, followed by ultrasonic-assisted casting and T8 heat treatment. A multiscale modeling approach combining ProCAST and Cellular Automata was established to simulate dendritic growth, solute distribution, and particle–matrix interactions. The results indicate that the introduction of TiC/TiB 2 suppresses macro-segregation of Cu, promotes heterogeneous nucleation, and refines the microstructure. Compared with Al Cu alloy, the grain size was reduced by 92.7% in the as-cast state. The tensile strength increased by 14.6%, reaching 543 MPa, while the elongation increased from 8.4% to 9.4%. A dendrite growth model was established based on the diffusion blocking effect of nanoparticles. Quantitative analysis revealed that TiC/TiB 2 particles inhibited dendritic growth, reducing the growth rate from 14.2 mm/s to 7.3 mm/s. Strengthening mechanism analysis confirms that Orowan strengthening is dominant (60.2%), followed by thermal mismatch (33.6%) and grain refinement (6.2%). This work significantly enhances the strength–ductility synergy of Al–Cu alloys by incorporating TiC/TiB 2 micro–nano particles, while establishing a multiscale simulation framework to systematically elucidate the interaction mechanisms between particles and solute transport behavior.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Jiang et al. (2026) studied this question.

synapsesocial.com/papers/69a760b6c6e9836116a2db96https://doi.org/10.1016/j.matdes.2026.115605