May 7, 2026International Journal of Electrochemical Science1 citationsOpen Access

Preparation and electrochemical performance of (La, Mg)₂Ni₇ hydrogen storage alloy as a function of sintering time

View Full Paper
TZTianming ZhaoYZYuyang ZhouCLChenyao Liu

Key Points

  • To investigate the effects of sintering time on the phase structure and electrochemical performance of (La, Mg)₂Ni₇ hydrogen storage alloy.
  • Vacuum powder sintering of LaNi₂.₃ and MgNi₁.₅₅ as intermediate alloys.
  • Sintering was conducted at 800℃ with varying times.
  • Electrochemical analysis of the resultant alloy was performed.
  • Alloy consisted of La 1.5 Mg 0.5 Ni 7 -type, La 2 MgNi 9 -type, and LaNi 5 -type phases.
  • Optimal performance at 4 hours sintering time: C max = 360.23 mAh/g, S 100 = 72.39%, HRD 900 = 91.35%.
  • Increased sintering time leads to magnesium volatilization and decomposition of La 1.5 Mg 0.5 Ni 7 phase.

Abstract

The (La, Mg)₂Ni₇ hydrogen storage alloy was prepared by vacuum powder sintering with using LaNi₂.₃ and MgNi₁.₅₅ as intermediate alloys. This study shows the effects of sintering time at 800℃ on the phase structure and chemical properties of the (La, Mg) 2 Ni 7 hydrogen storage alloy. The results show that the alloy consisted of the La 1.5 Mg 0.5 Ni 7 -type, La 2 MgNi 9 -type, and LaNi 5 -type phases, and increasing sintering time promote the formation of the LaNi 5 -type phase. Research findings have indicated that appropriately extending the sintering time can increase the alloy's maximum electrochemical capacity (C max ), improves its cycle stability(S 100 ), and enhance its high-rate discharge ability (HRD). For example, the alloy sintered for 4 hours exhibited optimal performance, with C max = 360.23 mAh/g, S 100 = 72.39%, and HRD 900 = 91.35%. It is concluded that as sintering time increases, there is excessive volatilisation of magnesium, which leads to the decomposition of the La 1.5 Mg 0.5 Ni 7 phase, resulting in an increase in the LaNi 5 phase. Electrochemical analysis of the alloy revealed that the alloy's high-rate performance is depended on the combined influence of I₀ and D₀, and exhibited a trend of initial improvement followed by deterioration. • Phase evolution is governed by Mg volatilization during sintering • Optimal performance is achieved at a sintering time of 4 h • Maximum discharge capacity reaches 360.23 mAh g⁻¹ • High-rate performance is controlled by both I₀ and hydrogen diffusion • Sintering time effectively tunes phase structure and electrochemistry

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Zhao et al. (2026) studied this question.

synapsesocial.com/papers/69fbefef164b5133a91a4002https://doi.org/10.1016/j.ijoes.2026.101397
Ask AI
Helpful
Bookmark
Share
View Full Paper

Also Consider

Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context:

  1. 1Effect of Step-wise Sintering Temperature on the Phase Structure and Electrochemical Properties of (La, Mg)2Ni7 Superlattice Hydrogen Storage Alloys2026
  2. 2Tailoring hydrogen storage performance of Mg-Mg<sub>2</sub>Ni alloys: synergistic effects of composition and phase formation with first-principles insights2025
  3. 3Non-stoichiometric Mg-Ni composites for hydrogen storage: role of in-situ Mg2Ni formation in enhancing hydrogen sorption performance2026
  4. 4Hydrogen storage properties of magnesium based alloys Mg<sub>67</sub>Ni<sub>(32-x)</sub>Nb<sub>1</sub>Al<sub>x</sub> (x = 1, 3, and 5) by using response surface methodology2024 · 7 citations
  5. 5Investigation of the Hydrogen Storage Performance of the LaNi₅ Alloy2026