February 6, 2026Journal of Mechanical Engineering and Manufacturing0 citationsOpen Access

CO2 Laser as a Sustainable Alternative for the Mitigation of Sanitary Ware Manufacturing Defects

View Full Paper
LDLuís M. P. DurãoRCRúben D. F. S. CostaAPArnaldo M. G. Pinto

Key Points

  • The aim is to explore the use of CO2 laser technology as a solution for repairing defects in ceramic sanitary ware instead of traditional methods.
  • Conduct experimental tests on ceramic sanitary ware defects using CO2 laser
  • Apply quantitative (colour difference reading, ANOVA) and qualitative analysis methods
  • Use optical microscope, SEM-EDS, and chemical analyses for defect assessment
  • Test various laser parameters including power and interaction time for optimal results
  • Best outcomes for white ceramic parts achieved between 50 and 70 W power levels
  • Optimal interaction time found to be 1 to 3 firings of 10 seconds each
  • Effective repair parameters for pinholes and fissures were identified at 50 W power and 30 seconds interaction

Abstract

The development of society through the centuries led to the improvement of healthcare and hygiene conditions throughout the world and, thus, the generalization of ceramic sanitary ware. Indeed, this industry possesses a huge financial impact on the global economy, employing thousands of people worldwide. In spite of their high production levels and increased efficiency, the sanitary ware manufacturing process is still characterized by some defects which make the commercialization of these products unfeasible. Currently, these flaws are rectified by a refiring in the kiln; however the defective parts occupy space intended for new ones to be produced and there is a high chance of new defects arising or the component to break due to the excessive heat of a second firing, hugely increasing the production costs. Accordingly, in this article a sustainable alternative is proposed, using a CO2 laser to repair only the defect area, thus leaving the remaining part untouched. Several laser parameters were tested in experimental tests of two different kinds of defects, using quantitative and qualitative analysis methods, through colour difference reading (with an ANOVA approach), and the optical microscope, SEM-EDS and chemical analyses, respectively. The best results considering defects provoked on a white coloured part were obtained with the manual firing for a laser power between 50 and 70 W, and an interaction time of 1 to 3 firings of 10 s each. These values apply for both pinholes and fissures, with a 50 W power and an interaction of 30 s being the best.

Ask AI
Helpful
Bookmark
Share
View Full Paper

Cite This Study

Durão et al. (2026) studied this question.

synapsesocial.com/papers/698585aa8f7c464f2300942dhttps://doi.org/10.53941/jmem.2026.100008
Ask AI
Helpful
Bookmark
Share
View Full Paper

Also Consider

Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context:

  1. 1CO2 laser processing of fused silica: a review of mechanisms, defect control and functionalization2026
  2. 2Systematic testing, verification and validation of laser treatments for unglazed earthenware affected by lichens and fungi biodeterioration2024
  3. 3Surface damage induced by micropores in transparent ceramics under nanosecond laser irradiation2024 · 4 citations
  4. 4Material migration and damage characteristics of fused silica optical surface treated by CO2 laser/short – pulse ultraviolet laser2024 · 18 citations
  5. 5Minimizing Defects in Additive Manufacturing and Laser Welding Through Energy Coupling Experiments and Dynamic Modelling2024