In the present study, the effects of electrode geometry and welding current on the tensile-shear strength, failure energy, fracture type, and joint microstructure were investigated during the RSW of ultra-high-strength MS1500 steel to high-strength low-alloy SPFC590 steel, both 1.2 mm in thickness. Three electrode geometries—designated as G0-6 mm, G0-8 mm, and A0—recommended for 1.2 mm sheets according to ISO 5821 were examined. It was found that in the G0-6 mm electrode geometry, which has the smallest contact area, excessive expulsion occurred at lower current levels compared to the other geometries. Consequently, this configuration resulted in lower maximum tensile-shear strength and failure energy values. The highest mechanical performance was achieved with the G0-8 mm electrode geometry, where the tensile-shear strength and failure energy were measured as 19.42 kN and 43.81 J, respectively. For the A0 electrode, although the maximum tensile-shear strength (19.68 kN) was comparable to that of the G0-8 mm geometry, the failure energy was approximately 7% lower (40.94 J). For all electrode geometries corresponding to maximum mechanical strength, a pull-out failure mode was observed, where the nugget region of the SPFC590 steel detached from the base metal and remained adhered to the ultra-high-strength MS1500 sheet.
Building similarity graph...
Analyzing shared references across papers
Loading...
Mehmet Okan Görtan
Ümit Türkmen
Metals
SHILAP Revista de lepidopterología
Hacettepe University
Kocaeli Üniversitesi
Building similarity graph...
Analyzing shared references across papers
Loading...
Görtan et al. (Tue,) studied this question.
www.synapsesocial.com/papers/69a75b7ec6e9836116a22e5e — DOI: https://doi.org/10.3390/met16020155